摘要 |
This polymer-composite modification product is obtained by means of performing a modification processing that is either a heating processing, irradiation processing, or electrical discharge processing on a mixture containing a macromolecule that satisfies the belowmentioned conditions 1 and 2, a metal complex having a molecular weight of at least 300, and carbon. (1) The nitrogen content is at least 1 mass%. (2) The mass reduction rate when heating from 300°C to 500°C in an inert gas atmosphere is within 50%. |