发明名称 PASTE FOR ELECTRODE FORMATION, TERMINAL ELECTRODE AND CERAMIC ELECTRONIC PART
摘要 <P>PROBLEM TO BE SOLVED: To provide paste for a terminal electrode, which has good sinterability, can keep good conductivity even when the paste is baked in the atmospheric environment, and allows the reduction in the manufacturing cost of ceramic electronic parts. <P>SOLUTION: The paste for electrode formation includes, as metal components, noble metal and base metal. As to the noble metal components, the paste includes (1) silver or (2) a combination of silver and palladium. As to the base metal components, the paste includes at least one of (3) a combination of copper and nickel, in which the content of nickel with respect to a total of copper and nickel is 10-80 mass%, and (4) a combination of copper and indium, in which the proportion of indium to a total of copper and indium is 0.3-8 mass%. The proportion of the noble metal to the base metal is 4-50 mass%. <P>COPYRIGHT: (C)2012,JPO&INPIT
申请公布号 JP2012033291(A) 申请公布日期 2012.02.16
申请号 JP20100169619 申请日期 2010.07.28
申请人 TDK CORP 发明人 INOUE YUKARI;YANAGIDA MIYUKI;ABE TOSHIYUKI
分类号 H01B1/20;H01G4/12;H01G4/252;H01G4/30 主分类号 H01B1/20
代理机构 代理人
主权项
地址