摘要 |
PROBLEM TO BE SOLVED: To provide a method of manufacturing a ceramic electronic component by which delamination, cracks, and mounting nonconformity can be reduced. SOLUTION: A group Q of electrodes is formed by aligning square electrodes 61 on a ceramic dielectric layer 51 with prescribed intervals. Then an auxiliary dielectric layer 65 which fills up the spaces between the electrodes 61 and the surroundings of the group Q of electrodes is formed. The auxiliary dielectric layer 65 has grooves 66 composed of non-printed sections in the spaces G1 between the electrodes 61 and the surroundings of the group Q. The grooves 66 are obliquely extended outward from the corner sections of the electrodes 61. COPYRIGHT: (C)2005,JPO&NCIPI
|