发明名称 METHOD OF PRODUCING AND HARDENING OF STEEL AND IRON PARTS
摘要 FIELD: process engineering. ^ SUBSTANCE: invention relates to metallurgy. Consumable pattern surface is coated by paste pre-diluted in fluid and containing the following components in wt %: chromium diboride - 10-40; boron carbide - 35-80; fine graphite - 7-18; sodium fluoride - 1-5; ammonium chloride - 1-3. Said coat is dried in air unless solid crust. Dried consumable pattern is formed in specially shaped moulding box to be filled with day quartz sand, melt is teemed to produce casting with diffusion layer. ^ EFFECT: accurate sizes, higher wear and rust resistance, decreased surface roughness. ^ 1 cl, 1 tbl, 1 ex
申请公布号 RU2440869(C1) 申请公布日期 2012.01.27
申请号 RU20100145915 申请日期 2010.11.10
申请人 GOSUDARSTVENNOE OBRAZOVATEL'NOE UCHREZHDENIE VYSSHEGO PROFESSIONAL'NOGO OBRAZOVANIJA "ALTAJSKIJ GOSUDARSTVENNYJ TEKHNICHESKIJ UNIVERSITET IM. I.I. POLZUNOVA" (ALTGTU) 发明人 GUR'EV ALEKSEJ MIKHAJLOVICH;IVANOV SERGEJ GENNAD'EVICH;GUR'EV MIKHAIL ALEKSEEVICH;ZEMLJAKOV SERGEJ ANATOL'EVICH;GRESHILOV ANATOLIJ DMITRIEVICH;IVANOV ALEKSEJ GENNAD'EVICH
分类号 B22D27/18 主分类号 B22D27/18
代理机构 代理人
主权项
地址