发明名称 CERMET AND COATED CERMET
摘要 The present invention is to provide a cermet which comprising a hard phase which contains W and nitrogen, and comprises at least one selected from a carbide, nitride and carbonitride of a metal comprising Ti as a main component, and a binder phase comprising an iron group metal as a main component, wherein a W amount contained in the whole cermet is 5 to 40% by weight, an interfacial phase comprising a complex carbonitride with a larger W amount than a W amount of the hard phase being present between the hard phase and the hard phase, and when a W amount contained in the interfacial phase based on the whole metal element is represented by Wb (atomic %), and a W amount contained in the hard phase based on the whole metal element is represented by Wh (atomic %), then, an atomic ratio of Wb to Wh (Wb/Wh) being 1.7 or more, which is excellent in fracture resistance and wear resistance.
申请公布号 EP2407263(A1) 申请公布日期 2012.01.18
申请号 EP20100750847 申请日期 2010.03.10
申请人 TUNGALOY CORPORATION 发明人 TAMURA, KEITARO;TAKESAWA, DAISUKE;HARA, HIROKI;KITAMURA, KOZO;TANIGUCHI, YASURO;HAYASHI, KOJI;MATSUMOTO, AKIHIRO;CHO, SUNG-PYO
分类号 B23B27/14;C22C1/05;C22C29/04;C23C14/06;C23C16/30 主分类号 B23B27/14
代理机构 代理人
主权项
地址