A method for accelerating the curing of a polyarylene sulfide. The polyarylene sulfide is blended with a cure accelerator to form a mixture where the weight percentage of accelerator is between 0.2% and 15.0% of the total weight of the blend. The mixture is cured at 320oC or above for at least 20 minutes. The cure accelerator is a compound selected from the group consisting of ionomers, hindered phenols, polyhydric alcohols, polycarboxylates, and mixtures of the foregoing.