摘要 |
<p>The invention relates to a method for producing fuel from sewage sludge which is linked with heavy metals immobilization. The method is characterized in that, to the mixture of sewage sludge and coal, glauconite in the amount of 0,2-2% on sludge dry matter basis is added, preferably in the form of a sand and gluconite mixture, of a gluconite content of 45-55% in the amount of 0,4-4 % on sludge dry matter basis.</p> |