发明名称 |
METHOD FOR PRODUCING FERRITE |
摘要 |
Disclosed herein is a method for producing a ferrite which can achieve high efficiency even in a high frequency range. The method comprises the steps of: mixing barium nitrate (Ba(NO 3 ) 2 ), cobalt nitrate hexahydrate (Co(NO 3 ) 2 ·6H 2 O) and ferric nitrate nonahydrate (Fe(NO 3 ) 3 ·9H 2 O) at a ratio of 3:2:24 to form a liquid-phase mixture; co-precipitating the mixture with sodium hydroxide (NaOH) so as to be metalized; washing and drying the co-precipitated mixture; heat-treating the co-precipitated mixture; and adding aluminum oxide (Al 2 O 3 ) to the mixture. The method can provide a high-efficiency ferrite having reduced permittivity, permeability, dielectric loss and permeability loss. |
申请公布号 |
EP2320434(A4) |
申请公布日期 |
2011.12.21 |
申请号 |
EP20090806826 |
申请日期 |
2009.08.11 |
申请人 |
EMW CO., LTD. |
发明人 |
RYU, BYUNG HOON;SUNG, WON MO;KUM, JUN SIG |
分类号 |
H01F1/032;C01G49/00;C01G51/00;C04B35/26;C04B35/626;H01F1/34 |
主分类号 |
H01F1/032 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|