The present invention relates to a process for producing microcellulose comprising subjecting fibrous cellulosic material to acid hydrolysis at a temperature of at least 40°C and at a consistency of at least 8% on dry weight of the cellulose, wherein the amount of added acid is from 0.2 to 2%, preferably from 0.5 to 1.5% on dry weight of the cellulose.
申请公布号
WO2011154601(A1)
申请公布日期
2011.12.15
申请号
WO2011FI50527
申请日期
2011.06.07
申请人
AALTO UNIVERSITY FOUNDATION;DAHL, OLLI;VANHATALO, KARI;PARVIAINEN, KARI;SVEDMAN, MIKAEL
发明人
DAHL, OLLI;VANHATALO, KARI;PARVIAINEN, KARI;SVEDMAN, MIKAEL