发明名称 Materialbehandlung für verminderte Schneidenergie und verbesserte Temperaturkapazität von Honigwabendichtungen
摘要 The present invention provides for a method to reduce the strength of the honeycomb (42) of a jet turbine stator (6), increasing its machinability, with a resultant reduction in measured peak tooth temperature, while maintaining or even improving its high temperature capability, so as not to limit its operating environment. The air seal functionality is unaffected, and even improved in some instances. The machinability of the honeycomb (42) is increased by using a light element diffused into the honeycomb ribbon to produce the effect of reducing its strength and ductility while maintaining the environmental resistance needed. The present invention also includes the stator honeycomb produced by the foregoing method. <IMAGE>
申请公布号 DE60219235(T3) 申请公布日期 2011.12.15
申请号 DE2002619235T 申请日期 2002.04.26
申请人 GENERAL ELECTRIC CO. 发明人 WALLACE, THOMAS TRACY;THOLKE, BRENT ROSS
分类号 C23C10/08;C23C8/06;C23C8/08;C23C8/24;F01D11/12 主分类号 C23C10/08
代理机构 代理人
主权项
地址