摘要 |
<p>In a process for producing die-cast parts made of an aluminum alloy, the aluminum alloy is exposed to high shearing forces in a mixing and kneading machine, is removed as partially solid aluminum alloy with a predefined solids content, is transferred into a filling chamber of a die-casting machine and is introduced into a casting mold using a piston, wherein a solids content of the aluminum alloy in a working space of the mixing and kneading machine is set to a predefined solids content by cooling and heating the working space in a targeted manner.</p> |