The invention provides a thermoplastic elastomer composition that has an excellent balance between flexibility and heat resistance (creep resistance), shows little tackiness (stickiness) and is not deteriorated in design properties even when exposed to a high temperature. A thermoplastic elastomer composition (X) includes a propylene copolymer (A) satisfying all the requirements (A1) to (A3) described below, a crystalline polyolefin polymer (B) which is optional, and a styrene block copolymer (C). (A1) The Shore A hardness is in the range of 50 to 90. (A2) The copolymer gives a melting peak Tm in the range of 30 to 95°C, and the endothermic enthalpy ”H corresponding to the melting peak is in the range of 1.0 to 20 J/g. (A3) The molecular weight distribution Mw/Mn is in the range of 1.2 to 3.0. |