A method of fabricating a solar cell involves electroplating a Group IIB-VIA material as a first or sub-layer over a junction partner layer, and then forming a second layer, also of a Group IIB-VIA material over the sub-layer. Both the sub-layer and the second layer comprise Te. The electroplating is performed at relatively low temperatures, as for example, below 100° C. Forming the sub-layer by low temperature electroplating produces a small grained compact film that protects the interface between the sub-layer and the junction partner during the formation of the second layer. The second layer may be formed by physical vapor deposition or ink deposition. A solar cell has a first layer of a stoichiometric Group IIB-VIA material formed on a CdS film, and a second layer of a Group IIB-V1A material. Both the first and second layers contain Te. The first layer may comprise CdTe with a grain size small than 0.5 microns and the second layer may comprise CdTe with a grin size in the range of 1-5 microns.
|