摘要 |
PROBLEM TO BE SOLVED: To solve such a problem that a countermeasure is performed by a means for squeezing and depositing a liquid after addition of a dilution solution such as an elastomer to a pulp fiber since in a pulp fiber composite PP (polypropylene), air remained in the fibrillated fine fiber of the surface of the pulp fiber is separated at injection molding and is remained on the molded article as a bubble and the designability is outstandingly reduced, on the contrary, reduction of impact strength is brought.SOLUTION: In the method for manufacturing the pulp fiber reinforced resin, after in the state that the pulp fiber is convected/stirred with air, it is mixed while blowing a dispersion containing a low elastic elastomer, the pulp fiber obtained by removing the solvent used for the dispersion is kneaded with the thermoplastic resin to make the composite. |