摘要 |
Provided are a method of producing an elastic fiber, including the steps of: subjecting a raw material to melt extrusion with a spinning nozzle at 100 to 300° C.; cooling the fiber after the melt extrusion in a water bath at 0 to 50° C.; and winding the cooled fiber, in which a specific low-crystalline polypropylene is used as the raw material, and an elastic fiber having a core-sheath bicomponent structure, which is obtained by using a specific low-crystalline polypropylene.
|