发明名称 |
PROCEDURE FOR PROTECTION OF STRUCTURE PARTS OF METALS OR THEIR ALLOYS FROM MELT OF CHEMICALLY ACTIVE METAL |
摘要 |
FIELD: metallurgy. ^ SUBSTANCE: procedure for protection of structure parts of steel or titanium from melt of chemically active metal consists in positioning source part in pressure tight reservoir, in sealed reservoir vacuumising, in heating part at rate of 100C each 10 minutes to 400C, in introduction of carbon dioxide into sealed reservoir at amount of 0.5 g/mol per each 1 cm2 of surface of part and in production of oxy-carbide layer of thickness as high, as 0.05 mm on surface of chemically active metal. ^ EFFECT: raised chemical resistance of structure metals to melt of chemically active metal at high temperature during period of contact of structure metal or its alloy with melt of chemically active metal for over 1 hour. ^ 6 dwg, 1 tbl, 5 ex |
申请公布号 |
RU2429310(C2) |
申请公布日期 |
2011.09.20 |
申请号 |
RU20090102723 |
申请日期 |
2009.01.27 |
申请人 |
ROSSIJSKAJA FEDERATSIJA, OT IMENI KOTOROJ VYSTUPAET GOSUDARSTVENNAJA KORPORATSIJA PO ATOMNOJ EHNERGII "ROSATOM";FEDERAL'NOE GOSUDARSTVENNOE UNITARNOE PREDPRIJATIE "ROSSIJSKIJ FEDERAL'NYJ JADERNYJ TSENTR - VSEROSSIJSKIJ NAUCHNO-ISSLEDOVATEL'SKIJ INSTITUT EHKSPERIMENTAL'NOJ FIZIKI" - FGUP "RFJATS-VNIIEHF" |
发明人 |
SKRIPNIKOV VLADIMIR VASIL'EVICH;KUZNETSOV MIKHAIL VALER'EVICH;KOCHANOV JURIJ ANATOL'EVICH;AFANAS'EV VLADIMIR ALEKSANDROVICH;TECHKO LEONID LEONIDOVICH |
分类号 |
C23C8/28 |
主分类号 |
C23C8/28 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|