发明名称 METHOD FOR COATING A METAL CRUCIBLE ELEMENT WITH A MIXTURE OF GLASS AND CERAMIC
摘要 Angular sectors of a cylindrical wall of a crucible for vitrification of waste, built in steel and subject to high temperatures, are coated with a mixture of mainly glass and ceramic, the coating being subject to a heat treatment comprising a step between 650° C. and 850° C. so as to perform surface melting of the mixture filling the open porosity, improving dielectric strength and the cohesion of the coating, but without producing any excessive thermal expansion or oxidation of the substrate which would lead to fast flaking of the coating.
申请公布号 US2011217485(A1) 申请公布日期 2011.09.08
申请号 US200913129368 申请日期 2009.11.17
申请人 AREVA NC 发明人 BRUN PATRICE;BERARD GEOFFROY;LACOMBE JACQUES
分类号 C23C16/30;C23C16/50;C23C16/56 主分类号 C23C16/30