<p>A method for producing a high-strength coke comprising, when the temperature at which the weight loss speed, that is obtained by first differentiating the weight loss during elevating the temperature to 900°C at a rate of 3°C/min with respect to time, attains the maximum is defined as the maximum weight loss temperature, carbonizing a starting coke material that is prepared by adding a first binder supplement having a maximum weight loss temperature equal to or higher than 400°C and a second binder supplement having a maximum weight loss temperature lower than 400°C to a staring coal.</p> |