发明名称 |
Method and device for the continuous creation of a bainite structure in a carbon steel, particularly in a strip steel |
摘要 |
A method continuously creates a bainite structure in a carbon steel, especially a strip steel by austenitizing the carbon steel; introducing the austenitized carbon steel into a bath containing a quenching agent; adjusting the carbon steel to the transformation temperature for bainite and maintaining the transformation temperature for a certain period of time; and then cooling the carbon steel. The carbon steel stays in the bath until a defined percentage of the bainite structure relative to the total structure of the carbon steel has formed. Residues of the quenching agent are removed from the surface of the carbon steel by blowing the same off when the carbon steel is discharged from the bath, and the remaining structure components of the carbon steel are then transformed into bainite in an isothermal tempering station without deflecting the carbon steel at all.
|
申请公布号 |
US2011198786(A1) |
申请公布日期 |
2011.08.18 |
申请号 |
US201113066564 |
申请日期 |
2011.04.18 |
申请人 |
C.D. WAELZHOLZ GMBH;EBNER INDUSTRIEOFENBAU GMBH |
发明人 |
KAISER WERNER;HOEFINGHOFF HEINZ;JUNIUS HANS-TONI;HELLMANN MICHAEL;EBNER PETER;LOCHNER HERIBERT |
分类号 |
C21D9/54;C21D1/62;C21D9/00 |
主分类号 |
C21D9/54 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|