摘要 |
This invention provides a rubber composition being excellent in the workability during production and the heat resistance and high in the storage elastic modulus (G′) and small in the loss tangent (tan δ), which is formed by compounding 1-60 parts by mass of a low-molecular weight conjugated diene-based polymer (B) having a weight average molecular weight as measured through a gel permeation chromatography and converted to polystyrene of 10,000-200,000 and a vinyl bond content in a conjugated diene compound portion of not less than 40% based on 100 parts by mass of a rubber component (A) comprised of at least one selected from the group consisting of natural rubber, polyisoprene rubber, styrene-butadiene copolymer rubber, polybutadiene rubber and isobutylene isoprene rubber, wherein the rubber component (A) comprises natural rubber and/or polyisoprene rubber and a proportion of styrene units in total of the low-molecular weight conjugated diene-based polymer (B) is less than 5% by mass.
|