摘要 <p>PURPOSE: Soil pavement containing an environmentally-friendly material, a composition thereof, and a soil paving method using the same are provided to reduce environmental contamination and efflorescence by employing blast furnace slag and waste FRP that replace cement of general soil pavement. CONSTITUTION: A soil paving method comprises steps of: compacting aggregate 5~20cm thick using a roller and setting a metal mesh; dry-mixing weathered granitic soil, yellow soil, cement, blast furnace slag powder, waste FRP powder; filling mixing water in a vehicle equipped with an agitator, putting the composition in the agitator, supplying mixing water including a hardening agent, and agitating the mixture for over 5 minutes; placing the soil paving composition on a paving target place; compacting the placed composition and forming a pattern on the compacted surface; and covering vinyl on the completed pavement and curing for 3 days.</p>
申请公布号 KR101050382(B1) 申请公布日期 2011.07.19
申请号 KR20090107162 申请日期 2009.11.06
申请人 发明人
分类号 E01C7/00;C04B18/06;E01C21/00 主分类号 E01C7/00
代理机构 代理人
主权项
地址