摘要 <p>PURPOSE: A method for manufacturing clay bricks is provided to optimize the reduction of the deformation of the bricks through a sintering process by adjusting the mixing ratio, the sintering time, and the sintering temperature of decarburization slag. CONSTITUTION: A method for manufacturing clay bricks includes the following: Water is added to an admixture of 30-60 weight% of decarburization slag and 70-40 weight% of clay. The particle size of the decarburization slag is 50mm or less. The water and the admixture are mixed. A vacuum pugging process is implemented to shape bricks, and the shaped bricks are dried and sintered at a temperature between 1050 and 1150 degrees Celsius for 1 to 24hours.</p>