摘要 An iron-chromium-aluminum alloy having a long service life and exhibiting little change in heat resistance, comprising (as percentages by weight) 4.5 to 6.5% Al, 16 to 24% Cr, 1.0 to 4.0% W, 0.05 to 0.7% Si, 0.001 to 0.5% Mn, 0.02 to 0.1% Y, 0.02 to 0.1% Zr, 0.02 to 0.1% Hf, 0.003 to 0.030% C, 0.002 to 0.03% N, a maximum of 0.01% S, and a maximum of 0.5% Cu, the remainder being iron and the usual steel production-related impurities.