摘要 |
The surface rough less of extruded wood composites and the die pressure in the extrusion process is improved by the incorporation of a process aid comprising fluoropolymer and a salt selected from the group consisting of potassium tetraborate, potassium pentaborate, potassium chloride, and the sodium, calcium or potassium salt of sulfate, pyrosulfate, persulfate, sulfite, phosphate, phosphite, and pyrophosphate.
|