摘要 |
Provided is a thermoplastic acrylic resin composition comprising a methacrylic resin (A) and a polyvinyl acetal resin (B) obtained by acetalizing a polyvinyl alcohol resin with an aldehyde having 4 or more carbon atoms and an aldehyde having 3 or less carbon atoms in which the total amount of the vinyl alcohol units acetalized with the aldehyde having 4 or more carbon atoms and the aldehyde having 3 or less carbon atoms is 65 to 85 mol % of all repeating units, and the molar ratio of the vinyl alcohol unit acetalized with the aldehyde having 4 or more carbon atoms to the vinyl alcohol unit acetalized with the aldehyde having 3 or less carbon atoms is from 90/10 to 0/100. Furthermore, provided are an article molded from the thermoplastic acrylic resin composition and a method of producing the thermoplastic acrylic resin composition comprising the steps of mixing a methacrylic resin (A) and a polyvinyl acetal resin (B), increasing the resin temperature to 160° C. or more, and then decreasing the resin temperature to 120° C. or less.
|