摘要 |
The invention provides a method of continuous casting for producing a slab excellent in surface quality by preventing formation of depressions and occurrence of cracking of a slab even in the case of producing a high Al steel having an Al content of 0.1% or more by continuous casting. At the time of continuous casting of a high-Al molten steel containing prescribed chemical components by using a mold powder, a powder containing T—CaO: 35 to 55%, SiO2: 10 to 30%, Al2O3: 4.0% or less (excluding 0%), MgO: 0.2 to 1.0%, Li2O: 7 to 13%, F: 7 to 13%, C: 10.5 to 14%, and inevitable impurities and satisfying 1.6≦̸[T—CaO]/[SiO2]≦̸5 and 0.2≦̸[Li2O]/[SiO2]≦̸1.1 is used as the mold powder, and operation is carried out while controlling the conditions such as the molten steel surface level fluctuation speed in the mold; the pouring angle of the molten steel in the width direction of the mold; the stroke in the amplitude; and the negative strip time tN defined by a prescribed relational expression.
|