摘要 |
PURPOSE: A method for fabricating textile containing tannin is provided to emit far infrared ray and anion. CONSTITUTION: A method for fabricating textile containing tannin comprises: a step of dipping the textile in 1-8 wt% of clean washing agent and 92-99 wt% of purified water and boiling at 60-110°C for 40-60 minutes to remove fat and foreign materials(S10); a step of stirring 96-97 wt% of crude tannin liquid, 2-2.5 wt% of mineral, and 0.1-1 wt% of pure silver at 18-32°C for 10-25 minutes to form a mixture(20)(S20); a step of dipping a textile in the mixture at 20-30°C for 20-30 minutes to contain the mixture into twisted yarn of the textile(S30); a step of performing S30 step to form a polymeric film; and a step of dipping the textile in a natural water containing mineral and carbonic acid for 1-5 hours to prevent discoloration(S40). |