发明名称 CRUMB RUBBER MODIFIED ASPHALT WITH IMPROVED STABILITY
摘要 The present invention relates to a method for producing a crumb rubber modified asphalt comprising the steps of: a) heating a pre-selected quantity of asphalt to a temperature of between about 325°F to 55O°F; b) adding crumb rubber and a mineral acid to the heated asphalt with stirring; and c) blowing air through the asphalt, crumb rubber and mineral acid mixture.
申请公布号 CA2780744(A1) 申请公布日期 2011.04.21
申请号 CA20102780744 申请日期 2010.10.13
申请人 INNOPHOS, INC. 发明人 MARTIN, JEAN-VALERY
分类号 C08L95/00;C08K5/51;C08L21/00;C09D195/00;E01C3/02 主分类号 C08L95/00