A solution (10) including a solvent and a monomer is coated on an area of a surface (16) of a piezoelectric member (12) such that the solution (10) flows into one or more defects (18). At least some of the solvent is removed to form a monomer film (20) within a defect (18), and the monomer film (20) is polymerized within the defect to form a polymer film (22) within the defect (18).
申请公布号
WO2011046537(A1)
申请公布日期
2011.04.21
申请号
WO2009US60358
申请日期
2009.10.12
申请人
HEWLETT-PACKARD DEVELOPMENT COMPANY, L.P.;MARDILOVICH, PETER;VANDER PLAS, HUBERT A.;ULMER, KURT M.
发明人
MARDILOVICH, PETER;VANDER PLAS, HUBERT A.;ULMER, KURT M.