摘要 |
Process for manufacturing a self-sealing elastomer composition, wherein the process comprises the following steps: firstly a masterbatch comprising at least one diene elastomer and a thermoplastic plasticizing hydrocarbon resin with a content greater than 30 phr is manufactured by compounding these various components in a mixer at a temperature or up to a temperature called the “hot compounding temperature” which is above the softening point of the hydrocarbon resin; and then at least one crosslinking system is incorporated into the masterbatch thus prepared, by compounding everything, in the same mixer or in a different mixer, at a temperature or up to a maximum temperature which is kept below 100° C., in order to obtain said self-sealing composition, and wherein at least one liquid plasticizer having a glass transition temperature (Tg) below −20° C. is furthermore incorporated in an amount of less than 60 phr into said masterbatch or into said composition. |
申请公布号 |
EP2310444(A2) |
申请公布日期 |
2011.04.20 |
申请号 |
EP20090777385 |
申请日期 |
2009.07.23 |
申请人 |
SOCIETE DE TECHNOLOGIE MICHELIN;MICHELIN RECHERCHE ET TECHNIQUE S.A. |
发明人 |
PIALOT, FREDERIC;FOMBELLE, DAMIEN;VOGE, BOZENA;MERINO LOPEZ, JOSE |
分类号 |
C08K3/06;B29C73/16;B29L30/00;B60C19/12;C08J3/20;C08J3/22;C08J3/24;C08K3/04;C08K5/00;C08K5/01;C08K5/31;C08L7/00;C08L9/00;C08L21/00;C08L25/04;C08L45/00;C08L91/00;C08L97/00;C09K3/10 |
主分类号 |
C08K3/06 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|