发明名称 PROCESSES FOR REDUCING FLATNESS DEVIATIONS IN ALLOY ARTICLES
摘要 A process for reducing flatness deviations in an alloy article is disclosed. An alloy article may be heated to a first temperature at least as great as a martensitic transformation start temperature of the alloy. A mechanical force may be applied to the alloy article at the first temperature. The mechanical force may tend to inhibit flatness deviations of a surface of the alloy article. The alloy article may be cooled to a second temperature no greater than a martensitic transformation finish temperature of the alloy. The mechanical force may be maintained on the alloy article during at least a portion of the cooling of the alloy article from the first temperature to the second temperature.
申请公布号 WO2011037759(A2) 申请公布日期 2011.03.31
申请号 WO2010US48328 申请日期 2010.09.10
申请人 ATI PROPERTIES, INC.;SWIATEK, GLENN J.;BAILEY, RONALD E. 发明人 SWIATEK, GLENN J.;BAILEY, RONALD E.
分类号 C21D8/02;C21D7/13 主分类号 C21D8/02
代理机构 代理人
主权项
地址