A method of extracting Te and bismuth oxide and recovering byproduct comprises: leaching raw materials with a Te content of ≧1.8% by utilizing a leaching system containing H2SO4, Cl−, Br−, NH4+ and NaClO3, reducing leach solution with SO2 gas by precipitation method after separating impurities from it, washing with concentrated hydrochloric acid to obtain tellurium precipitation (18), purifying to obtain Te with a purity of higher than 99.99%. The filtrate produced is used for extracting Bi2O3 with a purity of higher than 99.99% when Bi content in the raw material is ≧2%. Acidic waste solution produced during the process could be returned to the leaching step for recycle.
|