摘要 |
A method for manufacturing a glass molding die includes forming a substrate by hardening a steel material containing 0.3 wt % or more and 2.7 wt % or less of carbon and 13 wt % or less of chromium, and further containing at least one additive selected from 0.5 wt % or more and 3 wt % or less of molybdenum, 0.1 wt % or more and 5 wt % or less of vanadium, and 1 wt % or more and 7 wt % or less of tungsten, and then tempering the steel material at a temperature of 400° C. or higher and 650° C. or lower, forming a surface coating layer composed of an amorphous Ni-P alloy on the surface of the substrate, and heating the surface coating layer thereby rendering the surface coating layer an eutectic structure composed of Ni and Ni3P. |