发明名称 METHOD FOR MANUFACTURING ENVIRONMENTAL BARRIER COATING USING SINTERING AID
摘要 <P>PROBLEM TO BE SOLVED: To provide a method for manufacturing an environmental barrier coating for protecting CMC from a high temperature steam environment which exists in a gas turbine engine. <P>SOLUTION: The method for manufacturing an environmental barrier coating 12 using a sintering aid consists of a step of applying a bond coat layer 14 to a ceramic component 10, a step of manufacturing a transition layer slurry by mixing at least water and a main transition material which consists of a rare earth bisilicate or a dope rare earth bisilicate, similarly, a step of manufacturing an outer layer slurry by mixing a rare earth monosilicate, also similarly, a step for manufacturing a flexible layer slurry by mixing BSAS or a rare earth dope BSAS, a step of applying at least any one or more of the transition layer slurry, the outer layer slurry and the flexible layer slurry, and a step of forming at least any one or more of the bond coat layer, a transition layer 16 and an outer layer 20 or a flexible layer 18 by sintering the component. <P>COPYRIGHT: (C)2011,JPO&INPIT
申请公布号 JP2011046596(A) 申请公布日期 2011.03.10
申请号 JP20100169897 申请日期 2010.07.29
申请人 GENERAL ELECTRIC CO 发明人 KIRBY GLEN HAROLD;BOUTWELL BRETT ALLEN;SUBIT JESSICA L
分类号 C04B41/89;C04B41/85;C04B41/87;F01D5/28;F01D25/00;F02C7/00;F23R3/42 主分类号 C04B41/89
代理机构 代理人
主权项
地址