Methods of manufacturing an active material capable of improving the discharge capacity of a lithium-ion secondary battery are provided. The first method of manufacturing an active material comprises a hydrothermal synthesis step of heating a mixture containing a lithium source, a phosphate source, a vanadium source, water, and a reducing agent to 100 to 195° C. under pressure; and a heat treatment step of heating the mixture to 500 to 700° C. after the hydrothermal synthesis step. The hydrothermal synthesis step adjusts the ratio [P]/[V] of the number of moles of phosphorus [P] contained in the mixture before heating to the number of moles of vanadium [V] contained in the mixture before heating to 0.9 to 1.2. The second method of manufacturing an active material comprises a hydrothermal synthesis step of heating a mixture containing a lithium source, a phosphate source, a vanadium source, water, and a reducing agent to 200 to 300° C. under pressure and adjusts the ratio [P]/[V] of the number of moles of phosphorus [P] contained in the mixture before heating to the number of moles of vanadium [V] contained in the mixture before heating to 0.9 to 1.5.
|