摘要 |
PROBLEM TO BE SOLVED: To provide a new MOR type metalloaluminosilicate with a metal introduced into a skeleton, and a method for producing the same, which is easily and industrially applicable. SOLUTION: Disclosed are the MOR type metalloaluminosilicate, wherein the metal is at least one selected from Ti, Ga, In, Sn and Zr, a molar ratio of the metal/Si is 0.005-0.2 and a molar ratio of Si/Al is≥25, the metalloaluminosilicate, wherein the metal is Ti, a molar ratio of Ti/Si is 0.05-0.2 and a molar ratio of Si/Al is≥100, and the metalloaluminosilicate, wherein the metal is Sn, a molar ratio of Sn/Si is 0.005-0.2 and a molar ratio of Si/Al is≥100. COPYRIGHT: (C)2011,JPO&INPIT
|