发明名称 PROCEDURE FOR RECOVERY OF TIGHTNESS IN FLOW STRING OF WELL
摘要 FIELD: oil and gas production. ^ SUBSTANCE: procedure for tightness recovery in flow string of well consists in successive pumping liquid glass and water solution of calcium chloride into isolation zone. Further, there is performed grout torqueing. First, there is pumped fringe of fresh water. Liquid glass and water solution of calcium chloride are pumped with fringes starting from fringe of water solution of calcium chloride. Buffer fringe of fresh water is pumped between each fringe. Water solution of calcium chloride has density 1.30-1.38 g/cm3. Volume ratio between water solution of calcium chloride and liquid glass in fringes is set from 1: 1 to 1: 3. Amount of fringes of water solution of calcium chloride and liquid glass is set not less, than 2. Fringes of water solution of calcium chloride and liquid glass are pressurised with process fluid of 1.00-1.18 g/cm3 density. The well is flushed with process fluid of 1.00-1.18 g/cm3 density and there is performed process conditioning during 2-4 hours. Buffer fringe of fresh water is pumped prior to grout pumping. Upon grout pumping grout is pressurised with process fluid of 1.00-1.18 g/cm3 density, the well is flushed with process fluid of 1.00-1.18 g/cm3 density and process conditioning is carried out for 24-28 hours. ^ EFFECT: increased reliability of tightness recovery procedure. ^ 1 ex
申请公布号 RU2412333(C1) 申请公布日期 2011.02.20
申请号 RU20100114944 申请日期 2010.04.15
申请人 OTKRYTOE AKTSIONERNOE OBSHCHESTVO "TATNEFT'" IM. V.D. SHASHINA 发明人 KHISAMOV RAIS SALIKHOVICH;RAKHMANOV AJRAT RAFKATOVICH;GALIEV TIMUR IL'DUSOVICH;ASLJAMOV AJDAR INGELEVICH;GALIMOV ZUL'FAT FAUZAROVICH
分类号 E21B33/13 主分类号 E21B33/13
代理机构 代理人
主权项
地址