摘要 |
<p>First, a box 5 molded from a resin is prepared such as to have a rectangular parallelepiped outer form with a pair of grooves on the bottom face and a semispherical recess 9. Subsequently, a photocurable resin agent 27 is applied to a bottom area 12 of the recess 10 in the box 5. Then, while a light transmitting mold 28 having a bottom face formed with a plurality of grating grooves arranged in a row along a predetermined direction is pressed against the applied resin agent 27, the resin agent 27 is cured by irradiation with light, so as to provide the area 12 in the recess 10 with the grating 29 formed with a plurality of grating grooves. Next, Al, Au, or the like is vapor-deposited so as to cover the grating 29, thereby forming a reflecting film 15. Then, a photodetector 4 is accommodated in a package 2. This can easily manufacture a highly reliable spectrometer.</p> |