摘要 |
The invention relates to gypsum mortar with expanded vermiculite added with citric acid and tartaric acid and to the method for obtaining same, containing the following elements in the following proportions: between 40% and 70% calcium sulphate; between 40% and 70% laminated expanded vermiculite; between 0.05% and 0.3% citric acid; between 0.05% and 1% tartaric acid; between 0.01% and 0.5% sodium or potassium citrate; and water q.s.p. 1000 ml, in which, for surface coating, the added vermiculite is obtained following treatment in a vertical furnace, which provides improved grain size and sheets of exfoliated vermiculite without water or air, and the mortar is provided with citric acid and tartaric acid, copper sulphate and sodium or potassium scitrate, with the water being added before the mixture is produced.
|