The invention relates to building and relates to a mineral mixture for waterproof coatings. The mineral mixture comprises, mass %: sodium nitrate – 0.10-0.25, calcium chloride – 0.10-0.25, sodium carbonate – 0.14-0.37, calcium carbide – 0.3-0.15, plasticizer – 0.02-0.07, rust solvent – 0.04-0.006, carbonate fine filler – 5.00-14.00, cement – 32.50-38.00, quartz sand – 61.08 – 45.50. The developed mixture is more cost-saving in terms of material costs. |