发明名称 |
METHOD OF PRODUCTION OF POROUS TITANIUM |
摘要 |
FIELD: metallurgy. ^ SUBSTANCE: 5 mcm-25 mcm fraction of titanium powder produced by carbonyl method is used as source material. Powder is placed into a moulding case, packed by vibration and sintered under condition of low vacuum 10 Pa-100 Pa at temperature 630-80C. ^ EFFECT: production of item of high porosity with high degree of pores size uniformity and high strength. ^ 3 cl, 3 dwg, 2 ex |
申请公布号 |
RU2407817(C2) |
申请公布日期 |
2010.12.27 |
申请号 |
RU20090110638 |
申请日期 |
2009.03.23 |
申请人 |
GOSUDARSTVENNOE OBRAZOVATEL'NOE UCHREZHDENIE VYSSHEGO PROFESSIONAL'NOGO OBRAZOVANIJA "URAL'SKIJ GOSUDARSTVENNYJ UNIVERSITET IM. A.M. GOR'KOGO" |
发明人 |
KISEEV VALERIJ MIKHAJLOVICH;NEPOMNJASHCHIJ ALEKSANDR SOLOMONOVICH |
分类号 |
B22F3/11;C22C1/08 |
主分类号 |
B22F3/11 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|