摘要 Low-loss ferrite comprising 100% by mass of main components comprising 47.1-49.3% by mol of Fe2O3, 20-26% by mol of ZnO, and 6-14% by mol of CuO, the balance being NiO, and 0.1-2% by mass (as SnO2) of Sn and 0.05-2% by mass (as Mn3O4) of Mn, and having an average crystal grain size of 0.5-3 μm.
申请公布号 US2010321140(A1) 申请公布日期 2010.12.23
申请号 US20080526138 申请日期 2008.02.06
申请人 HITACHI METALS, LTD. 发明人 TANAKA SATORU;TACHIBANA TAKESHI
分类号 H01F17/06;H01F1/10 主分类号 H01F17/06