发明名称 COPPER ALLOY AND METHOD FOR PRODUCING THE SAME
摘要 PROBLEM TO BE SOLVED: To provide a copper alloy excellent in both of strength and conductivity, specifically, having tensile strength exceeding 900N/mm<SP>2</SP>and the conductivity of 20%IACS or more, and a method for producing the same. SOLUTION: The copper alloy contains Ni of 3.3 mass% or more and 8.4 mass% or less, and Si of 0.6 mass% or more and 2.1 mass% or less, and the remainder is constituted of Cu and inevitable impurities, mass ratio (Ni/Si) of Ni and Si is 4.0 or more and 5.5 or less, and the size of an inclusion to be deposited in the copper alloy is 10 &mu;m or less. COPYRIGHT: (C)2011,JPO&amp;INPIT
申请公布号 JP2010242154(A) 申请公布日期 2010.10.28
申请号 JP20090091470 申请日期 2009.04.03
申请人 MITSUBISHI ELECTRIC CORP;MITSUBISHI ELECTRIC METECS CO LTD 发明人 ITO TAKEFUMI;KAWAMATA SUSUMU;KAWABATA TOSHIKAZU;IWASHITA YUMIKO;KURITA TOSHIHIRO
分类号 C22C9/06;C22F1/00;C22F1/08;H01B1/02 主分类号 C22C9/06
代理机构 代理人
主权项
地址