摘要 |
PURPOSE: The functional water and the manufacturing method thereof applying the negative ion mix the mineral with the application of the water and heat with the water molecule. The emission of the negative ion and far-infrared radiation is induced. In that way the functional water of the abundant mineral is manufactured. CONSTITUTION: The arcose sandstone and cleistogamic flower stone are mixed. In the mixed material as described above is the average Celsius temperature 800 or less, it is plasticized for 8 hours. The materials and fixed number are mixed. The raw material mixed as described above is mixed over 5 hours. |