发明名称 |
CORE/SHELL TYPE PD/FE2O3NANOPARTICLE, METHOD FOR PRODUCING THE SAME, AND FEPD/FE NANOPARTICLE OBTAINED BY USING THE SAME |
摘要 |
<P>PROBLEM TO BE SOLVED: To provide a Pd/Fe<SB>2</SB>O<SB>3</SB>nanoparticle which can give an FePd/Fe magnetic nanoparticle in which the formation of the coarsened part of Fe is suppressed, and individual particles are isolated by performing hydrogen reduction heat treatment, to provide a method for producing the same, and to provide an FePd/Fe magnetic nanoparticle in which the formation of the coarsened part of Fe is suppressed, and individual particles are isolated. <P>SOLUTION: The core/shell type Pd/Fe<SB>2</SB>O<SB>3</SB>b nanoparticle is composed of a Pd core phase and an Fe<SB>2</SB>O<SB>3</SB>shell phase in which a core/shell structure can be confirmed by evaluation according to at least one element analysis by a TEM image, a HAADF image or an EDX (Energy Dispersive X-ray Spectrometer), and in which the average Pd compositional ratio obtained by EDX is ≤50 atm%. The production method uses the core/shell type Pd/Fe<SB>2</SB>O<SB>3</SB>nanoparticle. The FePd/Fe nanoparticle is obtained by subjecting the core/shell type Pd/Fe<SB>2</SB>O<SB>3</SB>nanoparticle to hydrogen reduction heat treatment. <P>COPYRIGHT: (C)2010,JPO&INPIT |
申请公布号 |
JP2010189721(A) |
申请公布日期 |
2010.09.02 |
申请号 |
JP20090035685 |
申请日期 |
2009.02.18 |
申请人 |
TOYOTA MOTOR CORP;UNIV OF TSUKUBA |
发明人 |
SAKUMA NORITSUGU;KATO AKIRA;SHOJI TETSUYA;TERANISHI TOSHIJI |
分类号 |
B22F1/02;B22F9/22;B22F9/24;B82B1/00;B82B3/00;H01F1/00;H01F1/06 |
主分类号 |
B22F1/02 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|