发明名称 PROCEDURE FOR FORMING SELF-CALCINATING COAL ANODE OF ALUMINIUM ELECTROLYTIC CELL
摘要 FIELD: metallurgy. ^ SUBSTANCE: invention refers to non-ferrous metallurgy, particularly to procedures at maintenance of self-calcinating anode on aluminium electrolytic cells with upper current conductor at aluminium production. Procedure for forming self-calcinating coal anode of aluminium electrolytic cell consists in charging anode mass, in charging aluminium materials in form of granules, in re-setting steel anode pins at higher horizon of the coal anode, in extracting steel pins from a body of the coal anode, in charging metered amount of under-the pin mass on base of coke and pitch into a hole and in arranging pins into the anode hole. Aluminium granules are charged into under-the pin mass partially instead of pitch at amount of 30-60% of pitch weight. ^ EFFECT: reduced amount of binding out of pitch at maintaining fluidity of solid-liquid composite of not whole anode mass, but exclusively under-the pin anode mass.
申请公布号 RU2397277(C1) 申请公布日期 2010.08.20
申请号 RU20090124275 申请日期 2009.06.24
申请人 FEDERAL'NOE GOSUDARSTVENNOE OBRAZOVATEL'NOE UCHREZHDENIE VYSSHEGO PROFESSIONAL'NOGO OBRAZOVANIJA "SIBIRSKIJ FEDERAL'NYJ UNIVERSITET" 发明人 LEONOV VIKTOR VASIL'EVICH
分类号 C25C3/12 主分类号 C25C3/12
代理机构 代理人
主权项
地址