摘要 |
In the method for producing a bi-axially oriented thermoplastic resin film, the longitudinal draw ratio X in a longitudinal drawing step is in the range of from 2.8 times to 3.5 times, and the transverse draw ratio Y in a transverse drawing step is in the range of from 3.8 times to 4.8 times. The expression: X≧0.25Y+2.0+(T−(Tg+50))/400, is satisfied where T° C. represents the temperature of the thermoplastic resin film in the transverse drawing step in a tenter 28 and Tg° C. represents the glass transition temperature of the thermoplastic resin film.
|