摘要 |
<p><P>PROBLEM TO BE SOLVED: To provide ink for transparent conductive film formation which forms a good pattern shape by a coating method using an inkjet printer. <P>SOLUTION: The ink for transparent conductive film formation contains transparent conductive particles, a dispersant, a surface modifier and a solvent, wherein the content of the solvent is 40-99 wt.% relative to the total weight of the ink, the solvent is at least one selected from the group consisting of 2-methyl-2,4-pentanediol, diethylene glycol mono-2-ethylhexyl ether, ethylene glycol mono-2-ethylhexyl ether and dipropylene glycol methyl ether acetate, and a contact angle of the ink with a substrate is 5-10°. <P>COPYRIGHT: (C)2010,JPO&INPIT</p> |