摘要 |
Use of an iron-nickel-cobalt alloy in CFC mould construction comprising (in % by mass) Ni from 30 to 35%, Co from 3 to 6%, Al from 0.001 to 0.1%, Mn from 0.005 to 0.5%, Si from 0.005 to 0.5%, C max. 0.1%, balance Fe and constituents resulting from production, with the alloy having a mean coefficient of thermal expansion in the temperature range from 20 to 200 DEG C of <2.0 OE10<−6>/K.
|