发明名称 |
SURFACE PROTECTION METHOD FOR OPEN RACK TYPE CARBURETOR |
摘要 |
PROBLEM TO BE SOLVED: To provide a surface protection method for repairing a decreased part or an annihilated part of a clad layer for covering the surface of an open rack type carburetor and a non-clad part in which the clad layer does not exist. SOLUTION: Either one or both of the decreased or annihilated portion (an A-surface or B-surface) of the clad layer 10 and the non-clad part (a C-surface), and the clad layer 10 (a K<SB>O</SB>-surface) around them are treated so that the surface roughness (Rz) of the existing part and non-existing part of the clad layer is uniform and coarse, and then an aluminum-zinc alloy with a corrosion potential lower by 30-100 mV than the corrosion potential of the clad layer is sprayed to form a fused aluminum-zinc alloy sprayed layer thinner than the thickness of the initial clad layer. It is preferable to provide a form of the thickness of the clad layer being 150-1,000μm and a form of the surface roughness (Rz) after uniform roughening treatment being 100μm or more. COPYRIGHT: (C)2010,JPO&INPIT
|
申请公布号 |
JP2010151336(A) |
申请公布日期 |
2010.07.08 |
申请号 |
JP20080327511 |
申请日期 |
2008.12.24 |
申请人 |
SUMITOMO PRECISION PROD CO LTD;TOKYO GAS CO LTD |
发明人 |
SOTOIKE YOSHIAKI;HIRAYAMA TOSHIHIRO;TAMARU HIDEO;KIMOTO EMI |
分类号 |
F28F19/06;C23C4/02;C23C4/06 |
主分类号 |
F28F19/06 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|